CONCRETE
By the early 1990's, Japan has developed and used SCC.
Water 150-210
All the materials are placed in the mixer & mixed well
M2
(W/C=0.24) 59.73 82.07 3.63 4.08 5.84 6.52
M3
(W/C=0.25) 53.11 81.62 3.43 4.05 5.72 6.20
M4
(W/C=0.26) 52.53 81.29 3.40 3.99 5.46 5.86
M5
(W/C=0.27) 52.48 80.53 3.37 3.89 5.18 5.69
DISCUSSION ON TEST RESULTS
Based on the above experimental results, the observations are as follows:
T500 time, V-funnel time, T5 time and U-box values are decreases with
the increase of w/c ratio.
L-box value increases with the w/c ratio and Compressive strength,
tensile strength and flexural strengths are decreasing as the w/c ratio
increases.
2. Nan Su, K.C. Hsu, H.W. Chai. A Simple mix design method for self-compacting
concrete, cement and concrete Research 2001.
4. 4. M.S. Shetty. “Concrete technology (theory and practice), S. Chand & Company
LTD. 2002
5. IS 456-2000 Code of practice for plain and reinforced concrete (3rd revision)