Sei sulla pagina 1di 2

SARBOTTAM CMENT PVT.

LTD
Complain (Cracks) Resolution Checklist
Regd. No: 7689/067/068 Vat No: 304569937

Owner : Address: Date :


Suppliers : Concreting Date : Curing Date :
Engineer : ASM/SO : GM :
Cement Used : OPC PPC Structural Component : Beam Wall Others…….
Crack Location: Everywhere Corner/joint others……….

Leakage Through crack : Yes No Formwork Condition: Slurry Leakage in joints Others…
Compaction:
Curing Condition During Visit : Cured
Width of Cracks : Less than Types of Crack : Hairline cracking Plastics – shrinkage cracking
1mm crazing spelling
More than 1mm

Concrete Mix proportion( C:S:A) : Water quantity Used :


Types of Cracks Causes Prevention

Plastic Shrinkage Crack Hot, windy day. Being curing after the trowel application and
(Occur when water Late or inadequate the concrete has stiffened to the point where
evaporates too quickly form curing a wet jut bag would to leave an impression on
the surface.) the concrete.

Settlement cracks Did you observe any sign


of settlement of
foundations, poor
compaction of soil?
Yes No Others……
Excess water in the mix Raining during/after If there is excessive raining, there we should
concreting even stop concreting.
Others……..
Rich Mix
Other Observations :

Solution to this problem: