REBOUND HAMMER TEST (ASTM C 805-02)

Project Name: Date & Time Tested:

Structure/Area/Floor Level: Type of Formworks used:

Design Strength: Surface Characteristics:

Test Rebound Number Corrected Estimated


Location/Grid Line Hammer Orientation Average Remarks
No. 1 2 3 4 5 6 7 8 9 10 Average Strength (psi)

Note: Discrad readings differing from the average of 10 readings by more than 6 units and determine the average of the remaining readings. If more than 2 readings differ from the average by 6 units, discard the entire set of readings.
Refer to Figure 1 on the Rebound Hammer Methodology for the Conversion curve for the average compressive strength