There is not much in here, just follow standard etching process, get some Ferric Chloride and mix it with a reasonable
quantity of water and etch the board. Here too, using too strong of an etching agent can corrode off the undersides of the
toner and damage the tracks, specifically for thin lines so it is rather better using a lower concentration etching solution and
let it etch for longer.